main materialPine board, cutting machine, electric sander, Angle iron, tape measure, triangle, pencil, hand drill, rubber hammer, C-clamp, wood screws, hex screws, pencils, paint,...

180cm bed production?

main material

Pine board, cutting machine, electric sander, Angle iron, tape measure, triangle, pencil, hand drill, rubber hammer, C-clamp, wood screws, hex screws, pencils, paint, sandpaper, etc.

production procedure

Select the wood needed for the solid wood bed, then determine the size and size of the bed, and finally determine the height and shape of the bed.

1: Make the bottom frame:

First measure the size of their own room needs, and then determine their own solid wood bed size. Today I made a 180*200cm solid wood bed, the main frame and bed legs I fixed with Angle iron, this is very practical, you can locate the right Angle. Then I'll use the air gun to secure the keel one by one.

2: Bed frame wrap:

After the bottom frame is done, measure the actual length and width of the bed, and then cut the corresponding pine plank strip. Then the cut pine plate, nail on the bed frame, of course, need to apply a little glue. Today, the development of glue has been able to achieve the point where the glue is stronger than the wood itself.

3: Bed edge leveling:

Next, remove the jig of the bed frame and begin to make the bed edge, it is best to do the level here first. I can do the three sides of the bed, the other side of the back part does not need to do the bed. When the edge of the bed is done, the foot is 45 degrees, and each part should be made fine.

4: Install backrest:

First assemble a 180cm*70cm support board with pine wood, and then fix the support board on the bed frame, and finally wrap the edge with pine wood strips.

5: Make a nightstand:

In fact, it can not be said that the bedside table, on both sides of the bed were made a 40cm*50cm extension board. You can put lamps, cell phones, things like that. Can also be flexibly removed, on the one hand is more practical, on the other hand, I think it is also very beautiful after installation.

6: Grinding paint:

And finally, the sanding, my sanding method starts with number 80, then 120,180,280. 80 is very thick to quickly remove flaws and scratches, in addition to all the numbers are just to remove the traces left by the previous one, so the speed is very fast, very less sandpaper.

After polishing, see if the furniture has uneven places, leveling with putty, and grinding again to a flat state. Use the brush to pull the paint apart, spread it out, next to each other, not this and that. After the first brush, let it sit for two or three hours, and then apply the second brush.

seven

completion